Physical Properties Metric English Comments
Density 1.068 g/cc
0.03858 lb/in³
Saint-Gobain Chemfab® 2 Porous PTFE-Coated Glass
Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas..
Density 1.068 g/cc
0.03858 lb/in³
Cyclewood Solutions Xylomer™ XM2-FPC Sustainable Injection Molding Resin
100% biodegradable and compostable thermoplastic. The sustainable bio-based resin properties perform between polypropylene and polystyrene. Xylomer™ is modified lignin, an abundant, natural bypro..
Density 1.068 g/cc
0.03858 lb/in³
Dow Glycidyl Methacrylate
Glycidyl Methacrylate For Aliphatic Epoxy Polymers (Clear, colorless liquid)Information provided by Dow