Physical Properties Metric English Comments
Density 1.079 - 1.099 g/cc
0.03898 - 0.03970 lb/in³
ASTM D4052
BASF Palamoll® 656 Polymeric Plasticizer
Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro..