Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.112 g/cc | 0.04018 lb/in³ | |
Saint-Gobain Chemfab® 183 PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain SPECIALTY SERIES Belting Products:Dimensional Stability: Width rigidity as well as length stability is maintained by CHEMFAB Specialty Series belting in co.. |