Density 1.124 g/cc

@Temperature 210 °C
0.04061 lb/in³

@Temperature 410 °F
Solvay Chemicals Glycerol alpha monochlorohydrin
Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay
Density 1.124 g/cc
0.04061 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON SD000 PA12
LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive.