Polymer Property : Density = 0.0412 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Nylene® 601 Nylon 6, 50% RH, Extrusion Grade
Extrusion grade. Nylene 601 is the heat stabilized version of 600 which is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other app..
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66
Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan..
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (DAM)
Information provided by Ravago.
Density 1.14 g/cc
0.0412 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Lanxess Durethan® B 30 S FN40 000000 Nylon 6
PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Grupo Repol Dinalon® C1S25 PA6/PA66 Blend, Unreinforced
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Solvay TECHNYL® C 402 M PA6, Conditioned
Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high ..
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Solvay TECHNYL® PSB 286 PA6, Conditioned
Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl..
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Techmer ES HiFill® PA6 AF Colors
Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid FiberAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricateAppearance: Colors AvailableInformation provi..
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 E4 A1 Nylon 66
Availability: North AmericaForms: PelletsFeatures: High ViscosityInformation provided by TP Composites, Inc.
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Techmer ES Plastiblend® PA6/6 L UV BK Nylon 66
Availability: North AmericaForms: PelletsAdditive: UV Stabilizer and LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP MF006AS PP
LNP THERMOCOMP* MF006AS is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Density 1.14 g/cc
0.0412 lb/in³
Trelleborg Emerson & Cuming Stycast® A-312 One-Component General Purpose Encapsulant
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as ..
Density 1.14 g/cc
0.0412 lb/in³
Covestro Apec® HT KU 1-9371 High-Heat Polycarbonate
Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated ..
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
DSM Akulon® S223-D (Dry) Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
DSM Akulon® S223-F Nylon 66 (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.14 g/cc
0.0412 lb/in³
dry; ISO 1183
DSM Novamid® 2030A PA666
Film Extrusion, Extrusion, Extrusion Grade
Density 1.14 g/cc
0.0412 lb/in³
dry; ISO 1183
DSM Novamid® 2030J PA666
Film Extrusion, Extrusion, Extrusion Grade
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
EMS-Grivory Grivory® BG-15 HM PA6-GF15
Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop..
Density 1.14 g/cc
0.0412 lb/in³
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Density 1.14 g/cc
0.0412 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by ..
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
DSM Akulon® S223-EH Nylon 66 (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
EMS-Grivory Grivory® F 47 NL nat 6028 PA6
Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai..
Density 1.14 g/cc
0.0412 lb/in³
ISO data
BASF Capron® 5202CQ Blend HS Blend Nylon 66 (Dry)  (discontinued **)
Capron 5202CQ HS Blend is a heat stabilized, blended polyamide 6,6 injection molding homopolymer developed for fast molding cycles. It is also available in pigmented versions.Capron 5202CQ HS Blend..
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, Conditioned
Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr..
Density 1.14 g/cc
0.0412 lb/in³
ASTM D1928/D 1505
Borealis Low Sulfur™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Low Sulphur LE0595 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to me..