Density 1.202 g/cc
0.04343 lb/in³
Pyrotek ISOMAG® 70 Structural Insulation
Isomag® 70 is magnesia silicate based formulation provides insulating properties similar to calcium silicate with good strength and dimensional stability up to 1000°C. ApplicationsTorpedo cars La..