Physical Properties Metric English Comments
Density 1.214 g/cc
0.04386 lb/in³
ISO 1183
Stir SpA SG 55 ATC (PVC)
Application: Extrusion non-toxic seal for wood window and door framesInformation provided by STIR SpA
Density 1.214 g/cc
0.04386 lb/in³
Dow ISONATE™ 143L Modified MDI
ISONATE™ 143L modified MDI is a polycarbodiimide-modified diphenylmethane diisocyanate.Information provided by Dow
Density 1.214 g/cc
0.04386 lb/in³
Dow ISONATE™ 143L Modified MDI
ISONATE™ 143 is a polycarbodiimide-modified diphenylmethane diisocyanate. Liquid at room temperature, this product has a low viscosity and good storage stability down to 75°F. The polycarbodiimi..