Physical Properties Metric English Comments
Density 1.026 - 1.226 g/cc
0.03707 - 0.04429 lb/in³
RP-17617
Solvay RHODOLINE® OTE 500 Surfactant
Description: Open time additive for zero to low VOC paints.Identification: DEFOAMER BLENDAvailable in: Asia Pacific, Europe, Latin America and North America.Applications: RHODOLINE© OTE 500 is a..