Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.23 g/cc | 0.0446 lb/in³ | |
Sika Industry SikaFlex 221 Fast Cure Polyurethane Sealant/Adhesive Sika 221 SikaFlex Fast Cure Polyurethane Sealant/AdhesiveThis versatile product is the most popular adhesive/sealant. It is an excellent adhesive/sealant and can handle many light bonding applicatio.. |
|||
Density | 1.23 g/cc | 0.0446 lb/in³ | |
Sika Industry SikaFlex 201 Adhesive Sika 201 SikaFlex AdhesiveSikaflex 201 meets Federal Specification TT-S-00230C, Type II, Class A and ASTK C-920, Type S, Grade NS. 15 - 15 mm Cut-Off. Good non-sag. Available in black, white, gray, .. |
|||
Density | 1.23 g/cc | 0.0446 lb/in³ | |
Sika Industry SikaFlex 219 LM Low Modulus Polyurethane Sealant Sika 219 LM SikaFlex Low Modulus Polyurethane SealantThis is a high performance, low modulus polyurethane base, non-sag elastomeric sealant with excellent adhesion to a wide variety of substrates. M.. |