Polymer Property : Density = 0.04491 lb/in³
Polymer Property :
Density =
0.04491 lb/in³
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
1.243
g/cc
0.04491
lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12
LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber.