Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0450 g/cc | 0.00163 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Evazote® EV45CN Conductive Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0450 g/cc | 0.00163 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® LD45 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0450 g/cc | 0.00163 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® LD45FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0450 g/cc | 0.00163 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® MP45 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0450 - 0.0650 g/cc | 0.00163 - 0.00235 lb/in³ | ISO 845-88 |
Eurofoam Evacell XM 2001 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Density | 0.0450 g/cc | 0.00163 lb/in³ | |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |