Polymer Property : Density = 0.04501 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.246 g/cc
0.04501 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP REL22 PA 66
LNP* LUBRICOMP* REL22 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Electrically Conductive.
Density 1.246 g/cc
0.04501 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DX12411C PC
LNP* STAT-KON* DX12411C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.