Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.27 g/cc | 0.0460 lb/in³ | Yield Density |
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |