Physical Properties Metric English Comments
Density 1.278 g/cc
0.04617 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66
LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare