Physical Properties Metric English Comments
Density 1.295 g/cc
0.04678 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66
LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber.
Density 1.295 g/cc
0.04678 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66
LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber.