Polymer Property : Density = 0.0468 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0468 lb/in³
Lord Adhesives 370 Two Component Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Density 1.29 g/cc
0.0468 lb/in³
Mid-Mountain Materials THERMOSEAL® 2000 High Temperature Cement
Description: A family of high temperature resistant cements carefully formulated to withstand thermal expansion and contraction under fluctuating heat conditions. THERMOSEAL® THERMAL CEMENTS are ..