Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.04822 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.335 g/cc
0.04822 lb/in³
Calculated from weight of 10 oz/sy
Mid-Mountain Materials ARMATEX® SF10 Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
Density 1.335 g/cc
0.04822 lb/in³
Calculated from weight of 17 oz/sy
Mid-Mountain Materials ARMATEX® SF17 Industrial Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
Density 1.335 g/cc
0.04822 lb/in³
Calculated from weight of 17 oz/sy
Mid-Mountain Materials ARMATEX® SF17 Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
Density 1.335 g/cc
0.04822 lb/in³
Calculated from weight of 18 oz/sy
Mid-Mountain Materials ARMATEX® SF18 Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
Density 1.335 g/cc
0.04822 lb/in³
Calculated from weight of 18 oz/sy
Mid-Mountain Materials ARMATEX® FF18 Fluoroelastomer Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...