Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.434 g/cc @Temperature 50.0 °C |
0.05181 lb/in³ @Temperature 122 °F |
|
Solvay Chemicals A20 Chloroform Chloroform is a non-flammable product.EINECS Number: 200-663-8/CAS Number: 67-66-3/UN number: 1888Information provided by Solvay |
|||
Density | 1.434 g/cc @Temperature 50.0 °C |
0.05181 lb/in³ @Temperature 122 °F |
|
Solvay Chemicals E9000 Chloroform Chloroform is a non-flammable product.EINECS Number: 200-663-8/CAS Number: 67-66-3/UN number: 1888Information provided by Solvay |
|||
Density | 1.434 g/cc | 0.05181 lb/in³ | JIS-Z-8807 |
Denka VINYKON TS1007T PVC, S grade for window frame gaskets A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |