Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.47 g/cc | 0.0530 lb/in³ | |
Industrial Laminates/Norplex MC330 Cotton Fabric Description: Grade MC330 is a cotton cloth/phenolic resin composite which is specially processed to be used in cryogenic applications. Such applications include spacers for installation of liquid ox.. |