Physical Properties Metric English Comments
Density 1.473 g/cc
0.05322 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal
LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Density 1.473 g/cc
0.05322 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal (Asia Pacific)
LNP STAT-KON* KEP33 is a compound based on Acetal resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Density 1.473 g/cc
0.05322 lb/in³
ISO 1183
Stir SpA SR 80 2 (PVC)
Application: Primary type TI 1Information provided by STIR SpA