Polymer Property : Density = 0.05654 lb/in³
Polymer Property :
Density =
0.05654 lb/in³
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
1.565
g/cc
0.05654
lb/in³
ISO 1183
Lanxess Pocan® DP 7102 000000 PBT, 30% Mineral (discontinued **)
PBT, 30% mineral, injection molding, LDS