Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.51 - 1.71 g/cc
0.0546 - 0.0618 lb/in³
Molded
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound
BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
Density 0.270 - 1.71 g/cc
0.00975 - 0.0618 lb/in³
Average value: 0.767 g/cc Grade Count:9
Overview of materials for Thermoset Polyurethane Foam, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu..
Density 1.51 - 1.71 g/cc
0.0546 - 0.0618 lb/in³
Molded
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound
BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..