Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.745 g/cc @Temperature 30.0 °C |
0.06304 lb/in³ @Temperature 86.0 °F |
Liquid |
3M Novec™ 774 Engineered Fluid 3M™ Novec™ 774 Engineered Fluid is a clear, colorless and low odor fluid, and is one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high.. |