Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.986 g/cc | 0.07175 lb/in³ | |
Pyrotek Pyrocast ALFS Abrasion-Resistant Refractory Castable Pyrocast ALFS refractory is a high flow, fused silica castable. At low water levels (6.5-7%), Pyrocast ALFS exhibits outstanding flow characteristics.ApplicationsAluminum melting equipment Aluminum.. |
|||
Density | 1.986 g/cc | 0.07175 lb/in³ | |
Pyrotek TS-206 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Dark Red color. High compressive and flexural strength.Information provided by Pyrotek. |