Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.0693 g/cc | 0.074751 lb/in³ | |
Saint-Gobain Chemfab® 10 Anti-Static PTFE-Coated Glass Description: Chemfab® Anti-static Series is a high quality PTFE-coated glass fabric that can be used for release sheets, belting, or other applications requiring the dissipation of static electri.. |
|||
Density | 2.0693 g/cc | 0.074751 lb/in³ | |
Saint-Gobain Chemfab® 10 Premium PTFE-Coated Glass Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot.. |