Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0788 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.18 g/cc
0.0788 lb/in³
ISO 1183-1
Murtfeldt Murflor® Polytetrafluoroethylene
Murflor® materials are suited to use in applications that require an excellent resistance to chemicals and heating steam. Murflor®’s working range starts at -200°C and can extend to +260°C with..
Density 2.18 g/cc
0.0788 lb/in³
ISO.1183 DIN.53479
Omnia Plastica PTFE Polytetrafluoroethylene
A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features:Chemical: ..
Density 2.18 g/cc
0.0788 lb/in³
ASTM D792
3M Dyneon™ CC698 PTFE 20% Fiberglass/Carbon Filled  (discontinued **)
Product Form: Black, pelletized powder. Applications include valve seats.Data provided by Dyneon.
Density 2.18 - 2.24 g/cc
0.0788 - 0.0809 lb/in³
molded; ASTM D792
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide
PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne..
Density 2.18 - 2.22 g/cc
0.0788 - 0.0802 lb/in³
Momentive Performance Materials "PG" Pyrolytic Graphite
Pyrolytic Graphite (PG) is a unique form of graphite manufactured by decomposition of a hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is ne..
Density 2.18 g/cc
0.0788 lb/in³
Corning Vycor® 7913 UV-Transmitting Glass
Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to high temperatures.Excellent thermal shock resistanceTypical Applications:Halogen l..
Density 2.18 g/cc
0.0788 lb/in³
Corning Vycor® 7950 Red Glass
Used to reduce the light of quartz lamps (blocks most visible white light while transmitting IR). One specific use is blocking glare from heating units.Special Features:Superior optical qualityTigh..
Density 2.18 g/cc
0.0788 lb/in³
ASTM D792
Solvay Specialty Polymers Algoflon® F3140 X PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..
Density 2.18 - 2.21 g/cc
0.0788 - 0.0798 lb/in³
extruded; ASTM D792
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..
Copyright © lookpolymers.com All Rights Reserved