Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0791 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.19 g/cc

@Temperature 25.0 °C
0.0791 lb/in³

@Temperature 77.0 °F
Schott Glass 8230 Intermediate sealing glass
The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG.
Density 2.19 g/cc
0.0791 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific)
This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region.
Density 2.19 g/cc
0.0791 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific)
This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region.
Density 2.19 - 2.49 g/cc
0.0791 - 0.0900 lb/in³
Green
CeramTec Ceramtape A Alumina for Constrained Sintering
LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process..
Density 2.19 - 2.27 g/cc
0.0791 - 0.0820 lb/in³
BS2782:Pt6
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Density 2.19 - 2.27 g/cc
0.0791 - 0.0820 lb/in³
BS2782:Pt6
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
Density 2.19 - 2.27 g/cc
0.0791 - 0.0820 lb/in³
BS2782:Pt6
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Density 2.19 - 2.27 g/cc
0.0791 - 0.0820 lb/in³
BS2782:Pt6
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
Density 2.19 g/cc
0.0791 lb/in³
ASTM D792
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material
Excellent heat, wear, and chemical resistance; Good cryogenic properties; Can be abrasive running against soft metals at high surface speed; Excellent material for back-up rings Information ..
Density 2.19 - 2.22 g/cc
0.0791 - 0.0802 lb/in³
molded; ASTM D792
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..