Polymer Property : Density = 0.0823 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.28 g/cc
0.0823 lb/in³
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating
This phosphate-bonded, alumina coating system bonds exceptionally well to dense refractory ceramics, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C)