Polymer Property : Density = 0.0824 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.850 - 2.28 g/cc
0.0307 - 0.0824 lb/in³
Average value: 2.01 g/cc Grade Count:24
Overview of materials for Polytetrafluoroethylene (PTFE) Powder
This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..