Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwid.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0040 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0070 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0140 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0230 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0280 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0337 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0120 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series Premium 1.5MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series Premium 3MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries Ballotini® Impact Beads Ballotini® impact beads are microspheres are used for precise metal finishing of parts. They offer an environmentally safe and cost effective method for metal surface cleaning and finishing. Coars.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 931 Cordierite Mg-Al-Si Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mo-Sci Corporation GL-0191-S Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres that appear colorlessTypical applications of GL0191S glass microspheres include: grinding, mixing media, filter aids, filter media, and thermal expansi.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mo-Sci Corporation GL-0275-S Class VI Soda-Lime Spheres Appearance: Solid soda-lime glass microspheres with light green color in powder form.Typical applications of GL0275-S beads including: high temperature spacer material for gauge control, coating, fi.. |
|||
Density | 2.50 - 3.20 g/cc | 0.0903 - 0.116 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 584.072 Chromium Carbide-Nickel-Chromium 75-25 (Cr3C2-NiCr) |
|||
Density | 2.50 - 3.20 g/cc | 0.0903 - 0.116 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |
|||
Density | 2.50 g/cc @Temperature 25.0 °C |
0.0903 lb/in³ @Temperature 77.0 °F |
|
Schott ILLAX® Amber Pharmaceutical Glass Amber Glass Pharmaceutical primary packaging for oralia and solid dosageInformation provided by SCHOTT AG. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | Specification, After dried @ 110°C/24 hrs |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Density | 2.50 g/cc @Temperature 25.0 °C |
0.0903 lb/in³ @Temperature 77.0 °F |
|
Schott AR-GLAS® Soda Lime Silicate Glass Soda lime silicate glass, high dielectric constant, glass to metal seal, pharmaceutical primary packaging, general technical applicationInformation provided by SCHOTT AG. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Schott G018-163 Dental Glass Remarks: Sr- and F-containing, very low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Pr.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec 701 Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Ceradyne Ceralloy® 546-3E Boron Carbide Features:low porosityhigh puritysingle phaseApplications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Ceradyne Ceralloy® 546-4E Boron Carbide Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | Apparent |
Gouda Vuurvast SiC 90 Dense Refractory Brick Description: Very good thermal shock resistance, abrasion resistance as well as very good heat conductivity makes this SiC based brick very well suited for muffles as well as for applications under .. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
AGY VeTron® Glass Fiber Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.Information provided by AGY Holding Corp. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0060 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |