Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.61 g/cc | 0.0943 lb/in³ | |
Schott BG7 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Density | 2.61 g/cc | 0.0943 lb/in³ | |
Schott N-BALF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.61 - 2.76 g/cc | 0.0943 - 0.0997 lb/in³ | |
3M 7000 Series Copper Roofing Granule (Wausau) 3M Copper Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and treate.. |