Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.1083 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.999 g/cc
0.1083 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Density 2.999 g/cc
0.1083 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific)
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.