Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.049 g/cc | 0.1102 lb/in³ | |
Esstech Esstech DSS™ V-258-4107 Silinated Dental Glass Esstech DSS™ Glass features optimized levels of silane and improved hydrophobicity, properties which may result in improved adhesion & compatibility of the organic / inorganic surfaces in the compo.. |
|||
Density | 3.049 g/cc | 0.1102 lb/in³ | |
Esstech V-117-1075 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |
|||
Density | 3.049 g/cc | 0.1102 lb/in³ | |
Esstech V-117-1095 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |
|||
Density | 3.049 g/cc | 0.1102 lb/in³ | |
Esstech V-117-1112 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |
|||
Density | 3.049 g/cc | 0.1102 lb/in³ | |
Esstech V-117-1140 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |
|||
Density | 3.049 g/cc | 0.1102 lb/in³ | |
Esstech V-117-1190 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |
|||
Density | 3.049 g/cc | 0.1102 lb/in³ | |
Esstech Esstech DSS™ V-117-4107 Silinated Dental Glass Esstech DSS™ Glass features optimized levels of silane and improved hydrophobicity, properties which may result in improved adhesion & compatibility of the organic / inorganic surfaces in the compo.. |