Physical Properties Metric English Comments
Density 0.112 g/cc
0.00405 lb/in³
Typical Compression Density
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam
This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing with very basic tools such as a cup and stir stick. The components are low-viscosity stable li..
Density 0.112 g/cc
0.00405 lb/in³
Compressed Density
Northstar Polymers MPP-R07B Polyurethane Formulation
This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-..
Density >= 0.112 g/cc
>= 0.00405 lb/in³
Monmouth Rubber & Plastics Durafoamâ„¢ C41NBR Nitrile Rubber
Information provided by Monmouth Rubber & Plastics Corp.
Density 0.112 - 0.176 g/cc
0.00405 - 0.00637 lb/in³
Monmouth Rubber & Plastics Durafoamâ„¢ DK3131 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Density 0.112 g/cc
0.00405 lb/in³
Unifrax Fiberfrax® HSA (OF) Ceramic Fiber Paper
HSA paper is made from high surface area (HSA) fibers that contain a low percentage of unfiberized material. Use of this fiber results in a paper with lighter weight and extremely low thermal condu..
Density 0.112 g/cc
0.00405 lb/in³
Unifrax Fiberwall® Bonded 22 Bonded Module System
Fiberfrax Bonded modules and Hefty-Loc alloy steel hardware are the components of the Hefty-Loc module lining system. The Hefty-Loc system provides an insulation lining for a variety of heat proces..
Density 0.112 g/cc
0.00405 lb/in³
Unifrax Fiberwall® Bonded 30 Bonded Module System
Fiberfrax Bonded modules and Hefty-Loc alloy steel hardware are the components of the Hefty-Loc module lining system. The Hefty-Loc system provides an insulation lining for a variety of heat proces..
Density 0.112 g/cc
0.00405 lb/in³
Hexcel® HexWeb® HRH-327 - 3/8 - 7.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Density 0.112 g/cc
0.00405 lb/in³
Hexcel® HexWeb® HRP - 3/16 - 7.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Density 0.112 g/cc
0.00405 lb/in³
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Density 0.112 g/cc
0.00405 lb/in³
Molded density, ASTM D1622
Covestro Bayfill® EA 6003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Density 0.112 - 0.122 g/cc
0.00405 - 0.00441 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..