Polymer Property : Density = 0.122 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.122 - 0.125 g/cc
0.00442 - 0.00450 lb/in³
Mallard Creek Polymers Tychem® 3100D Yield Modifier Additive
Tychem® 3000/3100D is well suited, but not limited to, dry-cast pavers and blocks, SCC, HPC, pre-cast and down hole cementing. Tychem® 3000/3100D is compatible under the most extreme condition..