Density 3.38 g/cc
0.122 lb/in³
calculated from bulk density after subtracting pore volume
MarkeTech Repton 663 Mullite
Brand 663 features: Zirconia.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycle..
Density 3.37 g/cc
0.122 lb/in³
Schott N-SF6 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.37 g/cc
0.122 lb/in³
Schott N-SF6HT Glass
Information Provided by SCHOTT North America, Inc.
Density 3.37 g/cc
0.122 lb/in³
Corning 0159 Lead Barium Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated.
Density 3.38 g/cc
0.122 lb/in³
ASTM D792
Solvay Specialty Polymers Algoflon® 50 INOX PTFE; Stainless Steel Filled  (discontinued **)
Data provided by the manufacturer.50 wt.% Stainless Steel. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, a..