Physical Properties Metric English Comments
Density 3.52 g/cc
0.127 lb/in³
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
Density 3.51 g/cc
0.127 lb/in³
Schott N-LAK9 Glass
Information Provided by SCHOTT North America, Inc.