Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.58 g/cc | 0.129 lb/in³ | |
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 13%. |
|||
Density | 3.58 g/cc | 0.129 lb/in³ | |
Mateck Magnesium Oxide Substrate, MgO Substrate single crystals for superconductivity |
|||
Density | 3.57 g/cc @Temperature 25.0 °C |
0.129 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8650 Sealing Glass Sealing glass for molybdenum, free from Na and K, of high lead content Implosion diodesInformation provided by SCHOTT AG. |
|||
Density | 3.57 g/cc | 0.129 lb/in³ | |
Schott N-PSK53A Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.58 g/cc | 0.129 lb/in³ | |
Schott N-SK16 Glass Information Provided by SCHOTT North America, Inc. |