Physical Properties Metric English Comments
Density 3.86 - 3.94 g/cc
0.139 - 0.142 lb/in³
Sintered
Nabaltec GRANALOX® NM 9915 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Density 3.86 - 3.92 g/cc
0.139 - 0.142 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9922 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.85 g/cc
0.139 lb/in³
GBC Grade 99 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
Density 3.85 g/cc
0.139 lb/in³
ICE Al2O3 99.5
Data provided by the manufacturer, International Ceramic Engineering.
Density 3.84 g/cc
0.139 lb/in³
Schott KZFS12 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.86 g/cc
0.139 lb/in³
Schott N-PK51 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Density 3.84 g/cc
0.139 lb/in³
Schott N-LAK7 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.86 g/cc
0.139 lb/in³
Schott SF2 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.85 g/cc
0.139 lb/in³
CoorsTek StatSafe™ ADC Static Dissipative Alumina
Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes..
Density 3.84 g/cc
0.139 lb/in³
Anderman Ceramics EA995 Sintered Alumina, 99.5%
Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. ..
Density 3.86 g/cc

@Temperature 20.0 °C
0.139 lb/in³

@Temperature 68.0 °F
Solvay Chemicals (CsAlF-Complex) Cesium Fluoroaluminate
Low-melting-point flux for brazing aluminum.HS No.: 38109090 /CAS-No.: 138577-01-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appl..