Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.78 - 3.85 g/cc | 0.137 - 0.139 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9816 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |