Physical Properties Metric English Comments
Density 0.152 - 0.208 g/cc
0.00550 - 0.00752 lb/in³
Dry
Reade Advanced Materials Diatomaceous Earth (DE) (SiO2·nH2O)
Description: A naturally occurring mineral derived from microscopic in size fossilized remains of marine diatoms. It has high absorption, low bulk density and high brightness.A silica source in the ..
Density 0.152 g/cc
0.00550 lb/in³
ASTM D1056
Rogers Corporation Bisco® MF1 9575 - 75 Silicone, High Performance Foam, Indentation Force Material
MF1® 9575 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superi..
Density 0.152 g/cc
0.00550 lb/in³
ASTM D1056
ACC Magnifoam™ MF1-9575™ MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Density 0.152 g/cc
0.00550 lb/in³
Nominal Core Density
Unifrax Fiberfrax® Duraset® Flet
Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers i..