Density 4.65 g/cc
0.168 lb/in³
Typical
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4984
High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4984.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi..
Density 4.65 g/cc
0.168 lb/in³
Typical
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4987
High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4987.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi..
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + Annealed
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. ..
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®..
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 20% Elongated Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 20% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL..
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Elongated Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL..
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + Annealed
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. ..
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®..
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STOA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STOA (885°C/1hr/AC + 705°C/1hr/AC) condition. Other data below are typical of TIMETAL..
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Typical
This entry has typical property data. Other database entries for TIMETAL® 6-2-4-6 have tensile and fatigue data for specific sample conditions.High-Strength, Intermediate Temperature AlloyFeatures..
Density 4.65 g/cc
0.168 lb/in³
Typical
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4986
High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4986.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi..
Density 4.65 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 17 Titanium Alloy (Ti-5Al-2Sn-4Mo-2Zr-6Mo); Aged Billet/Bar
Features: High strength, deep hardenable forging alloy primarily for jet engines. Allows heat treatment to a variety of strength levels in sections up to 6 inches. Offers good ductility and toughnes..
Density 4.65 g/cc
0.168 lb/in³
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
Data provided by Allvac.Applications: Intermediate-temperature jet engine applications. Blades, discs, spacers, seals. Standard, rotor/premium grades.
Density 4.65 g/cc
0.168 lb/in³
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age
Data provided by Allvac.Applications: Compressor discs, heavy section forgings for gas turbine engine components. High tensile strength and good fracture toughness.
Density 4.64 g/cc
0.168 lb/in³
Typical
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Beta Forged + STA
This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the Beta Forged + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4..