Physical Properties Metric English Comments
Density 0.190 - 4.80 g/cc
0.00686 - 0.173 lb/in³
Average value: 1.49 g/cc Grade Count:273
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Density 4.00 - 4.80 g/cc
0.145 - 0.173 lb/in³
ASTM B212
H.C. Starck Amperit® 518.002 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Density 4.00 - 4.80 g/cc
0.145 - 0.173 lb/in³
ASTM B417
H.C. Starck Amperit® 518.059 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Density 3.80 - 4.80 g/cc
0.137 - 0.173 lb/in³
ASTM B417
H.C. Starck Amperit® 544.059 Dense Coated Tungsten Carbide-Nickel 83-17 (WC-Ni)