Physical Properties Metric English Comments
Density 0.125 - 0.175 g/cc
0.00452 - 0.00632 lb/in³
ISO 845-88
Eurofoam Porocell POR 303/B GR CR-Neoprene/NBR Foam
Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam..
Density 0.125 - 0.175 g/cc
0.00452 - 0.00632 lb/in³
ISO 845-88
Eurofoam Porocell POR 303/B RS CR-Neoprene/NBR Foam
Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam..
Density 0.125 - 0.175 g/cc
0.00452 - 0.00632 lb/in³
ISO 845-88
Eurofoam Porocell POR 303/B CR-Neoprene/NBR Foam
Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam..