Polymer Property : Density = 0.196 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 5.42 g/cc
0.196 lb/in³
MarkeTech Zinc Selenide:Tellurium (ZnSe:Te) Scintillator Crystal
ZnSe(Te) single crystals are characterized by the unique combination of high conversion efficiency, intrinsic luminescence in the red region of spectrum, high thermal and radiation stability; they a..
Density 5.42 g/cc
0.196 lb/in³
Ferro CF 7570 Low-Temperature Sealing
VITREOUS Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ther..