Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.605 g/cc | 0.2025 lb/in³ | |
MarkeTech Zinc Oxide (ZnO) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |