Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.74 g/cc | 0.207 lb/in³ | DIN EN 623-2 |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
Density | 5.72 g/cc | 0.207 lb/in³ | ASTM C20 |
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 5.72 g/cc | 0.207 lb/in³ | ASTM C20 |
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |