Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.2671 - 0.3114 g/cc | 0.009647 - 0.01125 lb/in³ | |
Saint-Gobain Chemfab® TCK® 1590 High-Strength Leno Weave Open Mesh Belting Material Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid .. |