Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.06 g/cc | 0.327 lb/in³ | |
Lucas-Milhaupt BRAZE 380 Characteristics:Braze 380 is a free-flowing, low temperature filler metal with excellent wetting of most ferrous and non-ferrous base metals, and is a good substitute for cadmium-bearing filler meta.. |
|||
Density | 9.04 g/cc | 0.327 lb/in³ | |
Lucas-Milhaupt BRAZE 403 Carbide Brazing Alloy Applications: Braze 403 is a good intermediate temperature brazing alloy for use on stainless steels, mild steels, cast and malleable irons and various nonferrous alloys. This alloy is particularly.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | |
Lucas-Milhaupt Silvaloy® A38T Brazing Alloy Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.06 g/cc | 0.327 lb/in³ | |
Indium Corp. Indalloy 59 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, bar and rings, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, cold reduced sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Density | 9.04 g/cc | 0.327 lb/in³ | |
Weartech International WT-694 Cobalt Hardfacing & Wear Resistant Alloy Information provided by Weartech International |
|||
Density | 9.06 g/cc | 0.327 lb/in³ | |
Wall Colmonoy WALLEX 40 Cobalt-Nickel Alloy Description: A cobalt-nickel alloy powder that forms deposits similar to those of Wallex 50, but softer. Finished with carbide tools and grinding.Methods of Application: Spraywelder, Fusewelder, PT.. |
|||
Density | 9.05 g/cc | 0.327 lb/in³ | at RT |
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |