Physical Properties Metric English Comments
Density 0.357 g/cc
0.0129 lb/in³
Free Rise Density
Northstar Polymers MSB-M25F Microcellular Foam based on High Performance Polyester Polyurethane
This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste..